Electronic Grade Gel Styrene-Based Mixed-bed Resin(Non-Regenerative)
for Ultrapure Water Deionization Sytem
International Equivalent Models:
Dower MR-3,AmberliteMB20,MR-450
TECH-INDEXES: | SPECIFICATIONS: |
Matrix: | Styrene-divinylbenzene copolymer |
Physical form: | Spherical beads |
Ionic form as shipped: | H+ | OH- |
Total bulk exchange capacity: | ≥1.7mmol/ml(Cation Resins) ≥1.3mmol/ml(Anion Resins) |
Moisture bulk density: | 0.69~0.76g/ml |
Ration of cation to anion resin: | 1:1.5 |
Chemical stability: | Insoluble in water, diluted acid nor in alkali |
PH: | 1~14 |
Maximum operating temperature: | 60ºC |
Minimum bed depth: | 700mm |
Operating linear velocity: | 8~20 m/h |
Packing Specification: 25L/Bag
NOTE:
During the process of synthesizing this resin, the ionic transition rate of H+ and OH- is quite high.
Also, exposure to air for a long time will cause this resin to absorb a large amount of carbon dioxide, which will affect the operational performance and usability of the resin. Therefore, once opened, it needs to be used as soon as possible, and the unused parts must be carefully sealed.
In addition, the product should neither be exposed to air nor direct sunlight.